MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: RT/duroid® 5880LZ filled PTFE composites are designed for exacting stripline and microstrip circuit applications. The unique filler results in a low density, lightweight material for high performance weight sensitive applications

The very low dielectric constant of RT/duroid 5880LZ laminate is uniform from panel to panel and is constant over a wide frequency range. Its low dissipation factor extends the usefulness of RT/duroid 5880LZ to Ku-band and above.

RT/duroid 5880LZ laminates are easily cut, sheared and machined to shape. They are resistant to all solvents and reagents, hot or cold, normally used in etching printed circuits or in plating edges and holes.
Available with a range of copper cladding options.

Features:

  • Lowest dielectric constant available
  • Low Z-axis CTE
  • Lightweight / low density
  • Uniform electrical properties over a wide frequency range
  • Lead free process compatible

Typical Applications:

  • Airborne Antenna Systems
  • Lightweight feed networks
  • Military Radar Systems
  • Missile Guidance Systems
  • Point to Point Digital Radio Antennas

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccASTM D792
Moisture Absorption at Equilibrium 0.22 %ASTM D570
Thickness 10.0 - 100 milRange of thicknesses available
Outgassing - Total Mass Loss 0.010 %TML; ASTM E595
 0.020 %WVR; ASTM E595
Collected Volatile Condensable Material 0.010 %ASTM E595
 
Mechanical PropertiesOriginal ValueComments
Peel Strength >= 4.00 pliCopper; IPC-TM-650 2.4.8
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.10e+13 ohm-cmCondition A; IPC 2.5.17.1
Surface Resistance 2.60e+12 ohmCondition A; IPC 2.5.17.1
Dielectric Constant 1.92 - 2.0
@Frequency 1e+10 Hz
Z direction; Process; IPC-TM-650 2.5.5.5
 1.96
@Frequency 8.00e+9 - 4.00e+10 Hz
Z direction; Design; Differential Phase Length Method
Dielectric Strength 285 V/milIPC-TM-650 2.5.6.2
Dissipation Factor 0.0019
@Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.3
 <= 0.0027
@Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 41.5 µm/m-°CZ-Direction; IPC-TM-650 2.4.41
 43.0 µm/m-°CY-Direction; IPC-TM-650 2.4.41
 44.0 µm/m-°CX-Direction; IPC-TM-650 2.4.41
Specific Heat Capacity 0.950 J/g-°Ccalculated
Thermal Conductivity 0.330 W/m-K
@Temperature 80.0 °C
Z direction; ASTM C518
Flammability, UL94 V-0
 
Descriptive Properties
Dimensional Stability2 - 3 mm/mX, Y direction; IPC-TM-650 2.4.39A
Thermal Coefficient of Dielectric Constant22 ppm/°CZ direction; IPC-TM-650 2.5.5.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate
Ultracor® UQF-95-1/4-3.0 Honeycomb Core Material
Covestro Bayblend® KL 1-1430 Polycarbonate/ABS Blend
3M Scotchcast™ 2123 Re-enterable Insulating Electrical Resin

PROGA972 / 138412

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.