MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP17HT-100 One Component Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Requires no mixing
  • Not premixed and frozen
  • Superb high temperature resistance
  • Highly dimensionally stable
  • Conducts heat while still being electrically isolating
  • Can be cast in thicknesses up to 1/2 inch
Product Description: Master Bond EP17HT-100 is a high performance, one part epoxy that combines easy handling with superb physical properties. The use of this epoxy is straightforward and simple. EP17HT-100 is not premixed and frozen and has unlimited working life at room temperature. It has a moderate viscosity with good flow properties, and can be used for potting and encapsulation in thicknesses up to ½ inch. Most importantly, EP17HT-100 cures in 60-90 minutes at 200-220°F, or 45-60 minutes at 275-300°F. Optimal properties are achieved with curing at 3-4 hours at 300°F followed by post curing at 350-400°F for a few hours, if possible. And, although the best properties are obtained by going with the higher temperature curing, the 200-220°F schedule still gives very good physical strength values along with first rate thermal conduction and electrical insulation numbers as well. It bonds well to metals, composites, ceramics, glass and many plastics. EP17HT-100 has superior chemical resistance to oils, fuels, acids, bases, water and many solvents. The service temperature range is -100°F to +500°F. EP17HT-100 is naturally yellow-tan, but other colors are available. Storing at 40-50°F is more than sufficient and freezing is not required nor recommended. EP17HT-100 is an excellent choice in aerospace, electronic, optical and other high-tech applications, where the blend of a non-mix system, a lower heat curing schedule and robust properties, especially temperature resistance, is desirable.

Product Advantages:

  • Single component; no mixing needed
  • Unlimited pot life at room temperature
  • Versatile cure schedules starting at 200-220°F
  • Readily flowable
  • Notable mechanical strength properties
  • Especially useful in applications involving more temperature sensitive substrates

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 40000 - 70000 cPthixotropic
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 6000 psi
@Treatment Temp. 93.3 °C
Tensile lap, Aluminum to Aluminum, 90 min cure at 200°F
 >= 8000 psi
@Treatment Temp. 121 °C
Tensile lap, Aluminum to Aluminum, 60 min cure at 250°F
 >= 10000 psi
@Treatment Temp. 149 °C
Tensile lap, Aluminum to Aluminum, Optimum cure: 4 min cure at 300°F plus post cure
Adhesive Bond Strength >= 1400 psi
@Treatment Temp. 93.3 °C
Tensile lap, Aluminum to Aluminum, 90 min cure at 200°F
 >= 2100 psi
@Treatment Temp. 121 °C
Tensile lap, Aluminum to Aluminum, 60 min cure at 250°F
 >= 2700 psi
@Treatment Temp. 149 °C
Tensile lap, Aluminum to Aluminum, Optimum cure: 4 min cure at 300°F plus post cure
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm90 min cure at 200°F
 >= 1.00e+15 ohm-cm60 min cure at 250°F
Dielectric Constant 3.5
@Frequency 60 Hz
Optimum cure: 4 min cure at 300°F plus post cure
 3.7
@Frequency 60 Hz
60 min cure at 250°F
 4.1
@Frequency 60 Hz
90 min cure at 200°F
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.580 - 0.720 W/m-K
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 149 °C
Optimum cure, plus post cure for a few hours at 350-400°F
 45.0 - 60.0 min
@Temperature 135 - 149 °C
 60.0 - 90.0 min
@Temperature 93.3 - 104 °C
Shelf Life 3.00 - 6.00 Month
@Temperature 4.44 - 10.0 °C
in original, unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP42HT-2AO Two Component, Thermally Conductive, Heat Resistant Epoxy
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Master Bond EP30AN Thermally Conductive Dimensionally Stable Epoxy System
Master Bond EP21TDC-2AO Flexibilized, Thermally Conductive Two Component Epoxy
Master Bond EP21TDC-2AN Two Component, Flexibilized, Highly Thermally Conductive, Electrically Insulating Epoxy Resin

PMASTM809 / 185402

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.