MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation profile and chemical resistance even with heat exposure to 650°F. Its glass transition temperature (Tg) is 225°C. This system is also has very low exotherm upon curing and can be used in castings and encapsulations well beyond ½ inch in thickness. The minimum curing temperature for EP17HT-LO is 300°F with faster cures attainable at higher temperatures. EP17HT-LO is 100% reactive and contains no solvents or diluents. EP17HT-LO bonds well to similar as well as dissimilar substrates such as metal, ceramics, plastics and composites. It has resistance to many chemicals such as acids, bases, salts, fuels, oils and many solvents. Shrinkage upon cure is minimal. It is serviceable from -80°F to +650°F. This system is tan in color. EP17HT-LO retains its electrical insulation properties, even at higher temperatures. It should be noted, in order to obtain the optimum properties, a post cure of 2-12 hours at 350°F is recommended. As mentioned above, EP17HT-LO meets NASA low outgassing specifications. It is widely used in a variety of applications in the aerospace, oil and chemical processing, optical, opto-electronic and specialty OEM industries.

Product Advantages:

  • Single component system; no mixing prior to use. Contains no solvents, diluents or volatiles
  • Easy application; only positive contact pressure required during heat cure
  • Good tensile, shear and compressive strength properties
  • Certified to NASA low outgassing standards
  • High temperature resistance. Staggering Tg

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Viscosity 15000 - 25000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 80
Tensile Strength at Break 10000 psi
Tensile Modulus 400000 - 450000 psi
Compressive Strength >= 20000 psi
Shear Strength 2300 psi
@Temperature 204 °C
 3200 psi
@Temperature 23.9 °C
tensile lap, aluminum to aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cm
@Temperature 204 °C
 >= 1.00e+15 ohm-cm
@Temperature 75.0 °C
Dielectric Constant 4.4
@Frequency 60 Hz,
Temperature 25.0 °C
 4.7
@Frequency 60 Hz,
Temperature 204 °C
Dissipation Factor 0.0080
@Frequency 60 Hz,
Temperature 25.0 °C
 0.018
@Frequency 60 Hz,
Temperature 204 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 650 °F
Minimum Service Temperature, Air -80.0 °F
Glass Transition Temp, Tg 225 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 1.50 hour
@Temperature 177 °C
 1.50 - 2.00 hour
@Temperature 149 °C
 2.00 hour
@Temperature 149 °C
plus 2-12 hrs at 350°F
Shelf Life 3.00 - 6.00 Month
@Temperature 4.44 - 7.22 °C
in original, unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Master Bond EP101HTX-3 One Component Thermally Stable Epoxy System
Master Bond EP112LS Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation
Master Bond EP15 High Tensile Strength One Component Epoxy

PMASTB304 / 149551

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.