MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: NSF Standard 61 Certified

Information provided by Lubrizol

Lubrizol acquired the Isoplast product line from Dow in 2009.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 92ASTM D648
Hardness, Rockwell R 124ASTM D648
Tensile Strength, Ultimate 10000 psiASTM D638
Tensile Strength, Yield 12000 psiASTM D638
Elongation at Break 30 %ASTM D638
Elongation at Yield 9.0 %ASTM D638
Tensile Modulus 280000 psiASTM D638
Flexural Strength 14000 psiASTM D790
Flexural Modulus 330000 psiASTM D790
Izod Impact, Notched 1.10 ft-lb/in
@Thickness 3.17 mm,
Temperature -40.0 °C
ASTM D256
 2.00 ft-lb/in
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
Dart Drop, Total Energy 68.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 270 °Funannealed; ASTM D648
 290 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 240 °Funannealed; ASTM D648
 280 °Fannealed; ASTM D648
Vicat Softening Point 297 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Yellow Index 40 %ASTM D1925
Transmission, Visible 88 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 238 - 260 °C
Mold Temperature 93.0 - 121 °C
Drying Temperature 127 - 138 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
Lubrizol Estane® 2102-90A Thermoplastic Polyurethane Elastomer
Chemours Viton® ETP-500 Fluoroelastomer (FKM)
Chemours Viton® Extreme™ ETP-600S Fluoroelastomer Compound

PDOW1395 / 30613

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.