MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 2214 Regular Gray One-Part Epoxy Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Metal Filled

Material Notes: One part epoxy adhesive is a structural strength product that eliminates the mixing and weighing of two-part systems. This product must be heat cured.

Aluminum filled heat curing (250°F, 121°C) structural adhesive of paste consistency. Can bond metals, glass and may plastics.

Viscosity is paste. Optimum cure takes 60 minutes at 121°C/250°F, 10 psi. Average T-Peel at 75°F (24°C) is 5 PIW; 180° peel tested on aluminum per ASTM D 1876-61T.

Information provided by 3M Adhesives Division.

Key Words: 3M Adhesives Division
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 2.80 MPa
@Temperature 177 °C
ASTM D1002-64
 10.3 MPa
@Temperature 121 °C
ASTM D1002-64
 20.7 MPa
@Temperature -55.0 °C
ASTM D1002-64
 31.0 MPa
@Temperature 24.0 °C
ASTM D1002-64
 31.0 MPa
@Temperature 82.0 °C
ASTM D1002-64
 
Processing PropertiesOriginal ValueComments
Processing Temperature 121 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC
Epoxy Novolac 27%, Carbon fabric 73%
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC

PMMA51 / 53398

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.