MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elix Polymers Elix™ 114 H ABS Polymer Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; ABS Polymer

Material Notes: High heat ABS copolymer modified with poly(styrene-co-maleimide) used to impart superior heat distortion resistance for PVC & ABS compounds. Physical form: white to slightly yellow powder.

Information provided by Elix Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.380 - 0.480 g/ccASTM D1895
Particle Size 125 - 500 µm>90%; ASTM D1921
Melt Flow 6.0 - 12 g/10 min
@Load 10.0 kg,
Temperature 220 °C
cm³/10 min MVR; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Izod Impact, Notched (ISO) >= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point >= 112 °CB50; ISO 306
 
Descriptive Properties
Hardness Hc30min. 90 N/nm²ISO 2039-1
Polybutadiene Content18-22%lab internal-IR
Residual Monomers (%)max. 0.1%lab internal-GC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elix Polymers ELIX PC/ABS 5130 Polycarbonate/ABS Alloy
Elix Polymers ELIX ABS P3H-AT Acrylonitrile Butadiene Styrene (ABS)
Elix Polymers ELIX ABS H701 Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, High Impact
Elix Polymers Elix™ Ultra HH 4115 PG ABS Polymer
Elix Polymers Cadon CG 28 ABS Copolymer

PELIX931 / 192525

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.