MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Wacker® Catalyst OL Release Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Product description: WACKER® CATALYST OL is a highly-active platinum complex used for the thermal curing of additioncrosslinking, solvent-based and solventless silicones.

Special features:

  • Very high and constant catalyst activity
  • Rapid curing of addition-crosslinking silicone systems
  • Miscible with silicones in all proportions
  • Solventless
  • Halogen-free, non-corrosive
  • Apart from platinum, WACKER® CATALYST OL does not contain any heavy metals
Application: WACKER® CATALYST OL is dissolved in a reactive silicone polymer, which is incorporated into the cured rubber during the curing process. Combined with DEHESIVE® silicone polymers, it is excellently suited for providing various substrates, such as paper and films with a silicone coating that exhibits release properties towards tacky products used in technical, health, hygiene and food sectors.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccDIN 51757
Viscosity 800 cPdynamic
 
Thermal PropertiesOriginal ValueComments
Flash Point 62.0 °CISO 2719
Ignition Temperature 400 °CDIN 51794
 
Component Elements PropertiesOriginal ValueComments
Platinum, Pt 1.0 %
 
Descriptive Properties
AppearanceClear to slightly turbid, oil liquid
Colorcolorless to yellowish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Wacker® TPR Silicone Release Agent
Wacker Wacker® TPD Silicone Release Agent
Wacker Wacker® TNE 50 Silicone Release Agent
Wacker Wacker® TN Silicone Release Agent
Wacker Wacker® Catalyst EM 454 Release Coating-Silicone Emulsion

PWACK9737 / 205266

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.