375-L Insulating Cement used specifically in the aluminum industry as a filler material and trough liner, 375-L Insulating Cement is a 1500°F product Typical Applications: - Insulating and Sealing: For kiln and furnace refractory crowns and domes, and flat suspended arches. Insulation of small steel pipe fittings<
- Leveling: For warped steel furnace shells prior to installing refractories. Finish coat over block insulation.
- Repairs: For damaged block and pipe insulation.
- Irregular Fill: For areas in refractory backup insulation where other types of insulation would be difficult to apply.
Advantages:- Easy to Use: Mix with water and apply with trowel or shovel.
- Reduce Inventory: Ideal for plant maintenance inventory to reduce number of items used for small jobs.
- Reduce Construction Costs: Eliminate field cutting of block insulations for insulating irregular areas
Information provided by BNZ Materials Inc. |