MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celanex® 5202 PBT, 15% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposure. A typical application for Celanex 5202 is oven handles.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccISO 1183
Moisture Absorption 0.170 %23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0060 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPa5mm/min; ISO 527-2/1A
Elongation at Break 2.5 %5mm/min; ISO 527-2/1A
Tensile Modulus 6100 MPa50mm/min; ISO 527-2/1A
Flexural Strength 150 MPaISO 178
Flexural Modulus 5300 MPaISO 178
Izod Impact, Notched (ISO) 4.40 kJ/m²ISO 180/1A
Charpy Impact Unnotched 15.0 kJ/m²ISO 179/1eU
 17.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 4.70 kJ/m²ISO 179/1eA
 4.50 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+16 ohm-cmIEC 60093
Surface Resistance 4.00e+15 ohmIEC 60093
Dielectric Constant 2.7
@Frequency 1e+6 Hz
IEC 60250
 2.7
@Frequency 100 Hz
IEC 60250
Dielectric Strength 17.0 kV/mmIEC 60243-1
Dissipation Factor 0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 42.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 73.0 µm/m-°CISO 11359-2
Melting Point 225 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 180 °CISO 75-1, -2
Glass Transition Temp, Tg 50.0 °CISO 11357-1,-2,-3
Flammability, UL94 HB
 HB
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 93.0 °Ccavity
 250 - 265 °Chot runner
Feed Temperature 230 - 250 °C
Zone 1 230 - 250 °C
Zone 2 235 - 255 °C
Zone 3 235 - 255 °C
Zone 4 240 - 260 °C
Die Temperature 250 - 265 °C
Melt Temperature 235 - 265 °C
Drying Temperature 120 - 130 °C
Dry Time 4.00 hour
Moisture Content <= 0.020 %
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® CR180A Thermoplastic Polyurethane
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane
Lubrizol Estane® 54611 Polyester-Based Thermoplastic Polyurethane
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer
Braskem F2022/0 LDPE Cast Film Extrusion Polyethylene

PHCQ075 / 178530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.