MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zenite® 6330 NC010 LCP (Extended Tabular Temperature Data)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes: Zenite® 6330 NC010 is a 30% mineral reinforced liquid crystal polymer resin having excellent toughness and a heat deflection temperature of 245°C.

Celenese acquired the Zenite product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.63 g/ccASTM D 792
Density 1.64 g/ccISO 1183
Filler Content 30 %
Linear Mold Shrinkage, Flow 0.00 cm/cm
@Thickness 3.17 mm
ASTM D955
 0.00 cm/cm
@Thickness 2.00 mm
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 3.17 mm
ASTM D955
 0.0065 cm/cm
@Thickness 2.00 mm
ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPaISO 527
Tensile Strength, Ultimate 48.0 MPa
@Temperature 150 °C
ASTM D 638
 56.0 MPa
@Temperature 120 °C
ASTM D 638
 125 MPa
@Temperature 23.0 °C
ASTM D 638
 200 MPa
@Temperature -40.0 °C
ASTM D 638
Elongation at Break 5.0 %ISO 527
 2.5 %
@Temperature 150 °C
ASTM D 638
 3.2 %
@Temperature 120 °C
ASTM D 638
 4.0 %
@Temperature 23.0 °C
ASTM D 638
Tensile Modulus 4800 MPa
@Temperature 150 °C
ASTM D 638
 10000 MPa
@Temperature 23.0 °C
ISO 527
 10500 MPa
@Temperature 23.0 °C
ASTM D 638
 11600 MPa
@Temperature -40.0 °C
ASTM D 638
Flexural Strength 145 MPa
@Temperature 23.0 °C
ISO 178
 42.0 MPa
@Thickness 3.17 mm,
Temperature 150 °C
ASTM D790
 50.0 MPa
@Thickness 0.800 mm,
Temperature 150 °C
ASTM D790
 51.0 MPa
@Thickness 3.17 mm,
Temperature 120 °C
ASTM D790
 60.0 MPa
@Thickness 0.800 mm,
Temperature 120 °C
ASTM D790
 127 MPa
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D790
 158 MPa
@Thickness 0.800 mm,
Temperature 23.0 °C
ASTM D790
 192 MPa
@Thickness 3.17 mm,
Temperature -40.0 °C
ASTM D790
 260 MPa
@Thickness 0.800 mm,
Temperature -40.0 °C
ASTM D790
Flexural Modulus 7100 MPa
@Temperature 23.0 °C
ISO 178
 3300 MPa
@Thickness 3.17 mm,
Temperature 150 °C
ASTM D790
 3400 MPa
@Thickness 3.17 mm,
Temperature 120 °C
ASTM D790
 5000 MPa
@Thickness 0.800 mm,
Temperature 150 °C
ASTM D790
 5160 MPa
@Thickness 0.800 mm,
Temperature 120 °C
ASTM D790
 9600 MPa
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D790
 10700 MPa
@Thickness 3.17 mm,
Temperature -40.0 °C
ASTM D790
 13900 MPa
@Thickness 0.800 mm,
Temperature 23.0 °C
ASTM D790
 16700 MPa
@Thickness 0.800 mm,
Temperature -40.0 °C
ASTM D790
Izod Impact, Notched 1.60 J/cm
@Temperature 23.0 °C
ASTM D 256
Charpy Impact, Notched 0.900 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D 257
Surface Resistance >= 1.00e+16 ohmASTM D 257
Dielectric Constant 2.9
@Frequency 1e+6 Hz,
Temperature 23.0 °C
0.8mm (0.031in); ASTM D 150
 3.2
@Frequency 1e+6 Hz,
Temperature 23.0 °C
3.2mm (0.125in); ASTM D 150
 3.3
@Frequency 1000 Hz,
Temperature 23.0 °C
0.8mm (0.031in); ASTM D 150
 3.3
@Frequency 100 Hz,
Temperature 23.0 °C
0.8mm (0.031in); ASTM D 150
 3.6
@Frequency 100 Hz,
Temperature 23.0 °C
3.2mm (0.125in); ASTM D 150
 3.6
@Frequency 1000 Hz,
Temperature 23.0 °C
3.2mm (0.125in); ASTM D 150
 3.9
@Frequency 1e+9 Hz,
Temperature 23.0 °C
0.8mm (0.031in); ASTM D 2520 B
 3.9
@Frequency 1e+9 Hz,
Temperature 23.0 °C
1.6mm (0.062in); ASTM D 2520 B
 3.9
@Frequency 1e+9 Hz,
Temperature 23.0 °C
3.2mm (0.125in); ASTM D 2520 B
 4.0
@Frequency 1e+10 Hz,
Temperature 23.0 °C
1.6mm (0.062in); ASTM D 2520 B
 4.0
@Frequency 1e+10 Hz,
Temperature 120 °C
1.6mm (0.062in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 120 °C
0.8mm (0.031in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 120 °C
1.6mm (0.062in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 120 °C
3.2mm (0.125in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 150 °C
0.8mm (0.031in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 150 °C
1.6mm (0.062in); ASTM D 2520 B
 4.0
@Frequency 1e+9 Hz,
Temperature 150 °C
3.2mm (0.125in); ASTM D 2520 B
 4.0
@Frequency 1e+10 Hz,
Temperature 200 °C
1.6mm (0.062in); ASTM D 2520 B
 4.0
@Frequency 1e+10 Hz,
Temperature 150 °C
1.6mm (0.062in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 150 °C
3.2mm (0.125in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 200 °C
0.8mm (0.031in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 150 °C
0.8mm (0.031in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 120 °C
0.8mm (0.031in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 120 °C
3.2mm (0.125in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 23.0 °C
3.2mm (0.125in); ASTM D 2520 B
 4.1
@Frequency 1e+9 Hz,
Temperature 200 °C
1.6mm (0.062in); ASTM D 2520 B
 4.1
@Frequency 1e+9 Hz,
Temperature 200 °C
3.2mm (0.125in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 200 °C
3.2mm (0.125in); ASTM D 2520 B
 4.1
@Frequency 1e+10 Hz,
Temperature 23.0 °C
0.8mm (0.031in); ASTM D 2520 B
 4.2
@Frequency 1e+9 Hz,
Temperature 250 °C
3.2mm (0.125in); ASTM D 2520 B
 4.2
@Frequency 1e+9 Hz,
Temperature 200 °C
0.8mm (0.031in); ASTM D 2520 B
Dielectric Strength 26.0 kV/mm
@Thickness 3.20 mm,
Temperature 23.0 °C
Short time; ASTM D149
 41.0 kV/mm
@Thickness 1.60 mm,
Temperature 23.0 °C
Short time; ASTM D149
 49.0 kV/mm
@Thickness 0.800 mm,
Temperature 23.0 °C
Short time; ASTM D149
Dissipation Factor 0.0010
@Frequency 1e+10 Hz,
Temperature 23.0 °C
0.8mm (0.031in); ASTM D 2520 B
 0.0010
@Frequency 1e+10 Hz,
Temperature 23.0 °C
1.6mm (0.062in); ASTM D 2520 B
 0.0010
@Frequency 1e+10 Hz,
Temperature 23.0 °C
3.2mm (0.125in); ASTM D 2520 B
 0.0020
@Frequency 1e+9 Hz,
Temperature 23.0 °C
0.8mm (0.031in); ASTM D 2520 B
 0.0020
@Frequency 1e+9 Hz,
Temperature 23.0 °C
1.6mm (0.062in); ASTM D 2520 B
 0.0020
@Frequency 1e+9 Hz,
Temperature 23.0 °C
3.2mm (0.125in); ASTM D 2520 B
 0.0050
@Frequency 1e+10 Hz,
Temperature 120 °C
0.8mm (0.031in); ASTM D 2520 B
 0.0060
@Frequency 1e+10 Hz,
Temperature 120 °C
1.6mm (0.062in); ASTM D 2520 B
 0.0060
@Frequency 1e+10 Hz,
Temperature 120 °C
3.2mm (0.125in); ASTM D 2520 B
 0.0080
@Frequency 100 Hz,
Temperature 23.0 °C
3.2mm (0.125in); ASTM D 150
 0.0090
@Frequency 100 Hz,
Temperature 23.0 °C
0.8mm (0.031in); ASTM D 150
 0.0090
@Frequency 1e+10 Hz,
Temperature 150 °C
0.8mm (0.031in); ASTM D 2520 B
 0.0090
@Frequency 1e+10 Hz,
Temperature 150 °C
1.6mm (0.062in); ASTM D 2520 B
 0.0090
@Frequency 1e+10 Hz,
Temperature 150 °C
3.2mm (0.125in); ASTM D 2520 B
 0.012
@Frequency 1e+9 Hz,
Temperature 120 °C
0.8mm (0.031in); ASTM D 2520 B
 0.013
@Frequency 1000 Hz,
Temperature 23.0 °C
3.2mm (0.125in); ASTM D 150
 0.013
@Frequency 1000 Hz,
Temperature 23.0 °C
0.8mm (0.031in); ASTM D 150
 0.014
@Frequency 1e+9 Hz,
Temperature 120 °C
1.6mm (0.062in); ASTM D 2520 B
 0.014
@Frequency 1e+9 Hz,
Temperature 120 °C
3.2mm (0.125in); ASTM D 2520 B
 0.015
@Frequency 1e+10 Hz,
Temperature 200 °C
3.2mm (0.125in); ASTM D 2520 B
 0.017
@Frequency 1e+10 Hz,
Temperature 200 °C
0.8mm (0.031in); ASTM D 2520 B
 0.018
@Frequency 1e+10 Hz,
Temperature 200 °C
1.6mm (0.062in); ASTM D 2520 B
 0.018
@Frequency 1e+9 Hz,
Temperature 150 °C
0.8mm (0.031in); ASTM D 2520 B
 0.020
@Frequency 1e+9 Hz,
Temperature 150 °C
3.2mm (0.125in); ASTM D 2520 B
 0.026
@Frequency 1e+9 Hz,
Temperature 250 °C
3.2mm (0.125in); ASTM D 2520 B
 0.027
@Frequency 1e+9 Hz,
Temperature 200 °C
0.8mm (0.031in); ASTM D 2520 B
 0.028
@Frequency 1e+6 Hz,
Temperature 23.0 °C
3.2mm (0.125in); ASTM D 150
 0.029
@Frequency 1e+9 Hz,
Temperature 200 °C
3.2mm (0.125in); ASTM D 2520 B
 0.029
@Frequency 1e+6 Hz,
Temperature 23.0 °C
0.8mm (0.031in); ASTM D 150
Comparative Tracking Index 175 - 249 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°C
@Temperature 23.0 - 150 °C
ASTM E 228
CTE, linear, Transverse to Flow 22.0 µm/m-°C
@Temperature 23.0 - 150 °C
ASTM E 228
Melting Point 335 °CASTM D 3418
 335 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 245 °CISO 75-1/-2
 245 °CASTM D 648
Glass Transition Temp, Tg 120 °CASTM D 3418
UL RTI, Electrical 240 °C
@Thickness 1.50 mm
UL 746B
 240 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical with Impact 220 °C
@Thickness 1.50 mm
UL 746B
 220 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical without Impact 240 °C
@Thickness 1.50 mm
UL 746B
 240 °C
@Thickness 3.00 mm
UL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
UL94
 V-0
@Thickness 3.00 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
UL94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 355 °COptimum
 350 - 360 °C
Mold Temperature 80.0 °COptimum
 40.0 - 150 °C
Drying Temperature 150 °C
Dry Time 3 hourDehumidified Dryer
Moisture Content <= 0.010 %
 
Descriptive Properties
ColorNatural
Drying RecommendedYes
FeaturesAppearance, Pleasing Surface
 Arc Resistant
 Aromatic
 Chemical Resistance, Good
 Dimensional Stability, Good
 Flow, Good
 Heat Aging Resistance, Good
 Moisture Absorption, Low
 Platable
 Warpage, Low
FillerMineral filler
Flame Retardant - Halogen/Red Phosphorus FreeYes
FormsPellets
GenericLCP
Part Marking Code>LCP-MD30<ISO 11469
Polymer FamilyLCP
Polymer TypeLCP
ProcessingInjection Moldable
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Flame Retardant Resins
 Low Warp Resins
 Mineral Reinforced Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationLCP-MD30ISO 1043
UsesAutomotive Applications
 Automotive Electronics
 Automotive, Under the Hood
 Communication Applications
 Computer Components
 Connectors
 Electrical/Electronic Applications
 Parts, Engineering
 Parts, Thin-walled
 Printer Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese ZENITE 7130 LCP, 30% Glass Reinforced
Celanese Zenite® 6635 BK010 LCP
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Celanese ZENITE 5130L LCP, 30% Glass Reinforced

PHCQ540b / 89599

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.