MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
UCAR Carbon UCAR® PGW Pressure Molded Graphite
Categories: Carbon; Graphite

Material Notes: An economical low ash material with excellent thermal shock resistance, Grade PGW is well suited for the fine machining detail required in molds for casting metal shapes. Grade PGW is a molded version of Grade CBY with excellent internal structure.

Typical Applications:

  • Pressure casting molds
  • Centrifugal casting molds
  • Large diameter susceptors, furnace bases and covers
  • Heat shields

Tabular property data is typical across grain. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.63 g/cc
Particle Size <= 750 µm
Ash 0.12 %
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 1960 psi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000930 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.60 µm/m-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 130 W/m-K

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Poco Graphite ACF-10Q Industrial Grade Graphite
Poco Graphite ZXF-5Q Industrial Grade Graphite
UCAR Carbon UCAR® PGX Pressure Molded Graphite
UCAR Carbon UCAR® ATA Isostatic Molded Graphite
Poco Graphite AXF-5Q Industrial Grade Graphite

CGRAFT06 / 1172

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.