MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: DOWLEX® 2045.02 Polyethylene resin is a premier film resin for general packaging applications ranging from heavy duty applications to high speed, thin gauge applications. It contains high level of slip additive and medium level of antiblock additive. This resin complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2 (a) for food contact applications. The regulation should be consulted for complete details.

Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 g/cc
Thickness 25.0 microns
Melt Flow 1.0 g/10 min
@Load 2.16 kg
Melt flow ratio I10/I2 is 8.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 26.2 MPaMolded property
Film Tensile Strength at Yield, MD 11.0 MPa
Film Tensile Strength at Yield, TD 12.1 MPa
Tensile Strength, Yield 12.4 MPaMolded property
Film Elongation at Break, MD 520 %
Film Elongation at Break, TD 670 %
Elongation at Break 1000 %Molded value
Elmendorf Tear Strength MD 260 g
Elmendorf Tear Strength TD 640 g
Elmendorf Tear Strength, MD 10.4 g/micron
Elmendorf Tear Strength, TD 25.6 g/micron
Dart Drop 8.40 g/micron
Film Tensile Strength at Break, MD 51.4 MPa
Film Tensile Strength at Break, TD 37.2 MPa
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 106 °C
 
Optical PropertiesOriginal ValueComments
Haze 10 %
Gloss 55 %45°
 
Processing PropertiesOriginal ValueComments
Processing Temperature 226 °CFilm extrusion temperature
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Dow DOWLEX™ 2038 Linear Low Density Polyethylene
Dow DOWLEX™ 2267G Linear Low Density Polyethylene
Dow DOWLEX™ 2517 Linear Low Density Polyethylene, Narrow MW Distribution
Dow DOWLEX™ 2020G Linear Low Density Polyethylene

PDW431 / 34500

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.