MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polikim KESTAMID® GRF Polyamide 6, Graphite Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: Graphite and special lubricants are evenly dispersed in its entirety in this type of Polikim's cast polyamide. The material is dark grey colored. Kestamid®-GRF has a high degree of crystallinity and better hardness and compression strength properties compared to standard Kestamid®. It has a low coeffient of friction and a high degree of abrasion resistance. It has good weatherability and UV resistance properties and can be more easily mechanically machined compared to standard Kestamid®. It also can be used in higher temperatures compared again to the standard type.

Information provided by Polikim Polimer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
Water Absorption at Saturation 5.0 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ISO 868
Tensile Strength, Ultimate 750 kg(f)/cm²ISO 527
Elongation at Break >= 20 %ISO 527
Tensile Modulus 4100 MPaISO 527
Compressive Strength 950 kg(f)/cm²ISO 604
Compressive Modulus 3000 MPaISO 604
Izod Impact, Notched (ISO) 5.00 kJ/m²ISO 180
Charpy Impact Unnotched NBISO 179
Coefficient of Friction 0.15
K Factor (Wear Factor) 0.20[mg/km]
K (wear) Factor 120 x 10-8 mm³/N-M
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CISO 11359
Melting Point 220 °C
Maximum Service Temperature, Air 115 °Ccontinuous
 175 °Cshort term

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polikim KESTAMID® PA6G Polyamide 6
Polikim KESTAMID® HS Polyamide 6, Heat Resistant
Aluminum 1060-H16
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
Hippe PF CC 203 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet

PPOLIK015 / 99825

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.