MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow SPECFLEX™ NC 632 Polyol
Categories: Polymer

Material Notes: SPECFLEX™ NC 632 polyol is a specialty capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082-00-2 056449-05-9

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/cc
Viscosity Measure 1050 - 1250 cSt1050 - 1250 cStASTM D445
Maximum Moisture Content 0.0600.060wt% water; ASTM D203
ASTM Color <= 30<= 30APHA; ASTM D4890
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0500.050[mg KOH/g]; DOWM 100387-TE95A
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 200 °C>= 392 °FPensky Martens closed cup; ASTM D93
 
Descriptive Properties
Hydroxyl Number mg KOH/g30.5 - 34.5ASTM D4274

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow SPECFLEX™ NC 638 Polyol
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol
Dow SPECFLEX™ NC 630 Polyol
Dow VORANOL™ CP 4711 Polyol
Dow SPECFLEX™ NC 606 Polyol

PDOW1425 / 30643

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.