MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Europrene® SOL TH 2311 Styrene - Ethylene / Butylene Block Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Europrene® SOL TH 2311 is a linear block copolymer obtained by selective hydrogenation of styrene-butadiene-styrene block copolymers. The polymer is based on styrene and ethylene/butylene, where bound styrene content is 30%wt. A non-staining, TNPP free antioxidant system is added during the production process.

Key Features: Europrene® SOL TH 2311 is a linear triblock copolymer of low molecular weight. Europrene® SOL TH 2311 offers excellent thermal and color stability, along with very good adhesive properties even with high addition of resins and plasticizers.

Main Applications: Europrene® SOL TH 2311 is designed for high performance hot melt adhesives and polymer modification. Easily dispersible, SOL TH 2311 is also used in bitumen modification for roofing applications and technical compound.

Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 500 cPToluene sol., 20% wt; ASTM D1084
Melt Flow 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75ASTM D2240
Tensile Strength at Break 28.0 MPaASTM D412
Elongation at Break 550 %ASTM D412
300% Modulus 0.00500 GPa
@Strain 300 %
ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Europrene® SOL TH 2312 Styrene - Ethylene / Butylene Block Copolymer
Versalis Europrene® SOL TH 2314 Styrene - Ethylene / Butylene Block Copolymer
Versalis Europrene® SOL TH 2315 Styrene - Ethylene / Butylene Block Copolymer
Dynasol Solprene® 4302 Thermoplastic Rubber (SBS)
Dynasol Solprene® 9618 Multi-branched Thermoplastic Rubber (Multi-branched SBS)

PENG218 / 124612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.