MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Next Generation DOWLEX® IP-2580 resin is an improved processing linear low density polyethylene resin designed for excellent flow and stiffness with freezer grade impact properties. DOWLEX IP-2580 resin balances peak molecular weight with patented molecular weight distribution and a slightly higher density for better lid stiffness and handling. Produced under U.S. patent number 5,015,511 this resin provides the processability, stress crack resistance, and rigidity needed for down gauging a variety of lids. This material complies with FDA regulation 21 CFR 177.1520 c 3.1(a) for food packaging applications. The regulation should be consulted for complete details.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.933 g/cc0.0337 lb/in³
Viscosity  34000 cP
@Shear Rate 5000 1/s,
Temperature 190 °C
34000 cP
@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
 54000 cP
@Shear Rate 1000 1/s,
Temperature 190 °C
54000 cP
@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
 77000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
77000 cP
@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 80 g/10 min
@Load 2.16 kg
80 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 8.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 8.75 MPa1270 psi
Tensile Strength, Yield 11.8 MPa1710 psi
Elongation at Break 500 %500 %
Modulus of Elasticity 0.327 GPa47.4 ksiMolded Sample 2% Secant Modulus
Flexural Modulus 0.553 GPa80.2 ksi
Izod Impact, Notched (ISO) 32.0 kJ/m²
@Temperature -50.0 °C
15.2 ft-lb/in²
@Temperature -58.0 °F
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 101 °C214 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution
Dow DOWLEX™ 3010 Linear Low Density Polyethylene
Dow DOWLEX™ 2267G Linear Low Density Polyethylene
Dow DOWLEX™ 2503.10 Linear Low Density Polyethylene, Narrow MW Distribution
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution

PDW460 / 34529

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.