MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek PTB 2200 Structural Board
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes:

Applications

  • Caster tips
  • Small machined nozzles
  • Slotted caster tips

Advantages

  • High strength
  • Resistant to thermal shock
  • Easily machined
  • Non-wetting to molten non-ferrous metals
  • Low thermal mass
  • High temperature stability
  • Excellent insulation properties
  • Zero out-gassing

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.480 - 0.640 g/cc0.0173 - 0.0231 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00140 GPa0.203 ksiparallel to grain
 0.00620 GPa0.899 ksiperpendicular to grain
Compressive Strength 4.10 MPa595 psiThickness
 17.9 MPa2600 psiLength
 
Thermal PropertiesMetricEnglishComments
CTE, linear  0.900 µm/m-°C
@Temperature 20.0 °C
0.500 µin/in-°F
@Temperature 68.0 °F
thickness
 1.10 µm/m-°C
@Temperature 20.0 °C
0.611 µin/in-°F
@Temperature 68.0 °F
Length
Thermal Conductivity  0.0700 W/m-K
@Temperature 204 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 399 °F
 0.0900 W/m-K
@Temperature 425 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 797 °F
 0.110 W/m-K
@Temperature 630 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 1170 °F
 0.150 W/m-K
@Temperature 980 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1800 °F
Maximum Service Temperature, Air 1204 °C2199 °FContinuous
Shrinkage  1.6 %
@Temperature 1350 °C,
Time 86400 sec
1.6 %
@Temperature 2460 °F,
Time 24.0 hour
Linear
 10 %
@Temperature 1350 °C,
Time 86400 sec
10 %
@Temperature 2460 °F,
Time 24.0 hour
Thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek PT-10 Graphite
Pyrotek PROSILY G-11R Graphite Lubricant/Coating
Pyrotek PROSILY G-10R Graphite Lubricant/Coating
Pyrotek Pinnacle Thermocouple Protection Tubes O'-Sialon (Bonded Silicon Carbide) TCPT
Pyrotek PROSILY G-40W Graphite Lubricant/Coating

CPYRO082 / 1820

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.