MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP21AOHT Thermally Conductive, Electrically Insulating Two Component Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Excellent thermal conductivity
  • Room temperature curing
  • Convenient handling
  • Superior electrical insulation
  • Long working life
  • High temperature resistance
Product Description: Master Bond EP21AOHT is a two component, thermally conductive, electrically insulating epoxy adhesive, sealant, and coating combining an excellent performance profile, user friendly processing along with higher temperature resistance properties. It is very easy to use with a forgiving one to one mix ratio by weight or volume. It cures at ambient temperatures or more rapidly at elevated temperatures with the optimum schedule being overnight at room temperature followed by a few hours at 150- 200°F. Its most outstanding feature is its superior thermal conductivity while sustaining ample electrical insulation values. EP21AOHT adheres well to a wide variety of substrates, including metals, composites, ceramics, glass, rubbers and plastics. It offers sound chemical resistance versus water, oil and fuels. Other desirable properties include minimal shrinkage upon curing, a low coefficient of thermal expansion, standout dimensional stability, first rate compressive strength and a high modulus of elasticity. Another positive is the service temperature range of -60°F to +400°F. The color of Part A is gray and Part B is off-white. EP21AOHT has a broad combination of properties where top notch heat transfer and solid electrical insulation properties along with the other attributes mentioned above are needed, particularly in aerospace, electronic and specialty OEM type applications.

Product Advantages:

  • Convenient mixing: non-critical one to one mix ratio by weight or volume; smooth consistency
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required
  • High bonding strength to a wide variety of substrates
  • Low coefficient of expansion, very little shrinkage, superb dimensional stability
  • Outstanding thermal conductivity
  • Excellent electrical insulation properties

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 35000 - 65000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85 - 95
Tensile Strength 6000 - 7000 psi
Tensile Modulus 500000 - 550000 psi
Compressive Strength 20000 - 23000 psi
Adhesive Bond Strength 1000 - 1200 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.7
@Frequency 60 Hz
Dielectric Strength >= 400 V/mil
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.0 - 24.0 µm/m-°C
Thermal Conductivity 1.2981 - 1.4423 W/m-K
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 93.3 °C
 48.0 - 72.0 hour
@Temperature 23.9 °C
Working Life 90.0 - 120 minAfter mixing, 100 g batch
Shelf Life 6.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Cure ScheduleOvernight at 75°Fplus a few hours at 150-200°F, Optimum cure
Mixing Ratio1:1 by weight for volumeParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP42HT-2AO Two Component, Thermally Conductive, Heat Resistant Epoxy
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Master Bond EP30AN Thermally Conductive Dimensionally Stable Epoxy System
Master Bond EP21TDC-2AO Flexibilized, Thermally Conductive Two Component Epoxy
Master Bond EP21TDC-2AN Two Component, Flexibilized, Highly Thermally Conductive, Electrically Insulating Epoxy Resin

PMASTM817 / 185410

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.