MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exceed™ 1018CA Metallocene Polyethylene Resin (European Grade)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Exceed 1018 CA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018CA have outstanding tensile, puncture resistance and very good sealing properties. These superior properties together with excellent draw down make this a versatile polymer for mono layer and multi layer blown film applications.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Agricultural Film
  • Bag in a Box
  • Barrier Food Packaging
  • Blown Film
  • Blown Stretch Film
  • Bread Bags
  • Food packaging
  • Form Fill and Seal Packaging
  • Freezer Film
  • General Packaging
  • Heavy Duty Bags
  • Lamination Film
  • Multilayer Packaging Film
  • Overwrap Film
  • Packaging Films
  • Premium Trash Bags
  • Stand Up Pouches
  • Trash Bags

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ExxonMobil method
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 560 %560 %ASTM D882
Film Elongation at Break, TD 680 %680 %ASTM D882
Puncture Energy 4.29 J3.17 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 230 g230 gASTM D1922
Elmendorf Tear Strength TD 350 g350 gASTM D1922
Dart Drop Test 1400 g3.09 lbASTM D1709
Film Tensile Strength at Break, MD 82.7 MPa12000 psiASTM D882
Film Tensile Strength at Break, TD 68.3 MPa9900 psiASTM D882
1% Secant Modulus, MD 172 MPa25000 psiASTM D882
1% Secant Modulus, TD 179 MPa26000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 118 °C<= 244 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 3.0 %3.0 %ASTM D1003
Gloss 14 %14 %45°; ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade)
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade)
Aluminum A360.0-F Die Casting Alloy
Aluminum 360.0-F Die Casting Alloy

PEX99041 / 175277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.