MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 7050-T73511; 7050-T73510
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: 7050 has very high strength coupled with high resistance to exfoliation corrosion and stress-corrosion cracking, high fracture toughness, and fatigue resistance. This leads to applications in aircraft structures.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A97050; ISO AlZn6CuMgZr; Aluminum 7050-T73510; AA7050-T73511; Al7050-T73511
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.83 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 132500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 166Converted from Brinell Hardness Value
Hardness, Rockwell A 49.8Converted from Brinell Hardness Value
Hardness, Rockwell B 80Converted from Brinell Hardness Value
Hardness, Vickers 151Converted from Brinell Hardness Value
Tensile Strength, Ultimate 72.0 ksiAA; Typical
Tensile Strength, Yield 63.0 ksiAA; Typical
Elongation at Break 12 %
@Diameter 12.7 mm
AA; Typical
Modulus of Elasticity 10400 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.33
Fracture Toughness 26.4 MPa-m½average; S-L
 31.9 MPa-m½average; T-L
 45.1 MPa-m½average; L-T
Shear Modulus 26.9 GPa
Shear Strength 290 MPaCalculated value.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000430 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.7 µm/m-°C
@Temperature -50.0 - 20.0 °C
 23.5 µm/m-°C
@Temperature 20.0 - 100 °C
 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
 24.4 µm/m-°C
@Temperature 20.0 - 200 °C
 25.4 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.860 J/g-°C
Thermal Conductivity 155 W/m-KEstimated from other heat treatments.
Melting Point 524 - 635 °CFor homogeneous wrought material. Eutectic for nonhomogeneous wrought or as-cast material that has not been heat treated is 465ºC.
Solidus 524 °CFor homogeneous wrought material. Eutectic for nonhomogeneous wrought or as-cast material that has not been heat treated is 465ºC.
Liquidus 635 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 775 °F
Solution Temperature 890 °F
Aging Temperature 250 - 350 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 87.3 - 90.3 %As remainder
Chromium, Cr <= 0.04 %
Copper, Cu 2.0 - 2.6 %
Iron, Fe <= 0.15 %
Magnesium, Mg 1.9 - 2.6 %
Manganese, Mn <= 0.10 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.12 %
Titanium, Ti <= 0.06 %
Zinc, Zn 5.7 - 6.7 %
Zirconium, Zr 0.08 - 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 7050-T73651 plate
Aluminum 7050-T7451 (7050-T73651)
Aluminum 7050-T74
Aluminum 7050-T7651
Aluminum 7050-T73652 forgings

MA7050T735 / 9575

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.