MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: High flow PC/ABS material that can be used for automobile R/G door handle

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow  4.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
 35 g/10 min
@Load 10.0 kg,
Temperature 250 °C
35 g/10 min
@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103ASTM D785
Tensile Strength, Yield 48.1 MPa6970 psi50 mm/min; ASTM D638
Elongation at Break 25 %25 %50 mm/min; ASTM D638
Flexural Strength 65.7 MPa9530 psi2.8 mm/min; ASTM D638
Flexural Modulus 1.86 GPa270 ksi2.8 mm/min; ASTM D638
Izod Impact, Notched  3.92 J/cm
@Thickness 6.35 mm
7.35 ft-lb/in
@Thickness 0.250 in
ASTM D256
 5.39 J/cm
@Thickness 3.17 mm
10.1 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
@Thickness 6.40 mm
210 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 110 °C230 °FB/50; ISO R306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Flexalloy® 9605-70FR Polyvinyl Chloride, Elastomer
Covestro Bayblend® 2953 Polycarbonate + ABS Blend, Automotive Plating
Lotte Advanced Materials Infino® WP-1069 PC/ABS, Unreinforced
Lotte Advanced Materials Starex® WR-9120 J ASA, Unreinforced
Trinseo PULSE™ EXT 100 PC/ABS Engineering Resin

PSAMSU952 / 146769

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.