MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics THERM-A-GAP 580 Thermally Conductive Gap Filler
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: THERM-A-GAP™ 580 is a highly conformal, thermally conductive gap filler pad. The materials consist of an ultra-soft silicone elastomer filled with ceramic particles. THERM-A-GAP™ elastomers are used to fill air voids between PC boards or high temperature components and heat sinks, metal enclosures, and chassis. The exceptional conformability of these advanced materials enables them to blanket highly uneven surfaces, wetting out mating surfaces in order to efficiently transfer heat away from components.

Typical Applications: Telecommunications equipment; Consumer electronics; Automotive electronics (ECUs); LEDs, lighting; Power conversion; Desktop computers; laptops, servers; Handheld devices; Memory modules and Vibration dampening

Product Attributes: Best for molding complex parts and vibration dampening and Lowest outgassing

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.90 g/ccASTM D792
Thickness 20.0 - 200 milASTM D374
Deformation 7.0 %
@Thickness 2.54 mm,
Pressure 0.0689 MPa
0.75" diameter round probe with 0.75" diameter circular sample; Method 2
 7.0 %
@Thickness 3.17 mm,
Pressure 0.0345 MPa
0.5" diameter probe, 0.025 in/min rate; ASTM C165 MOD
 10 %
@Thickness 3.17 mm,
Pressure 0.0689 MPa
0.5" diameter probe, 0.025 in/min rate; ASTM C165 MOD
 12 %
@Thickness 2.54 mm,
Pressure 0.138 MPa
0.75" diameter round probe with 0.75" diameter circular sample; Method 2
 13 %
@Thickness 2.54 mm,
Pressure 0.0689 MPa
1" square probe with 0.5" diameter circular sample; Method 1
 17 %
@Thickness 2.54 mm,
Pressure 0.0000400 MPa
0.75" diameter round probe with 0.75" diameter circular sample; Method 2
 18 %
@Thickness 2.54 mm,
Pressure 0.138 MPa
1" square probe with 0.5" diameter circular sample; Method 1
 20 %
@Thickness 3.17 mm,
Pressure 0.172 MPa
0.5" diameter probe, 0.025 in/min rate; ASTM C165 MOD
 24 %
@Thickness 2.54 mm,
Pressure 0.414 MPa
0.75" diameter round probe with 0.75" diameter circular sample; Method 2
 25 %
@Thickness 2.54 mm,
Pressure 0.276 MPa
1" square probe with 0.5" diameter circular sample; Method 1
 30 %
@Thickness 3.17 mm,
Pressure 0.345 MPa
0.5" diameter probe, 0.025 in/min rate; ASTM C165 MOD
 30 %
@Thickness 2.54 mm,
Pressure 0.552 MPa
0.75" diameter round probe with 0.75" diameter circular sample; Method 2
 31 %
@Thickness 2.54 mm,
Pressure 0.414 MPa
1" square probe with 0.5" diameter circular sample; Method 1
 37 %
@Thickness 2.54 mm,
Pressure 0.552 MPa
1" square probe with 0.5" diameter circular sample; Method 1
 39 %
@Thickness 2.54 mm,
Pressure 0.689 MPa
0.75" diameter round probe with 0.75" diameter circular sample; Method 2
 40 %
@Thickness 2.54 mm,
Pressure 0.689 MPa
1" square probe with 0.5" diameter circular sample; Method 1
 43 %
@Thickness 2.54 mm,
Pressure 0.827 MPa
1" square probe with 0.5" diameter circular sample; Method 1
 46 %
@Thickness 2.54 mm,
Pressure 0.827 MPa
0.75" diameter round probe with 0.75" diameter circular sample; Method 2
Outgassing - Total Mass Loss 0.18 %TML; ASTM E595
Collected Volatile Condensable Material 0.050 %ASTM E595
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 45ASTM D2240
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Constant 8.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 200 V/mil
Dissipation Factor 0.010
@Frequency 1e+6 Hz
Chomerics Test
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µin/in-°FASTM E831
Specific Heat Capacity 1.00 J/g-°CASTM E1269
Thermal Conductivity 3.00 W/m-KASTM D5470
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -55.0 °C
Flammability, UL94 V-0E140244
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 MonthFrom date of shipment A; Chomerics
 24.0 MonthFrom date of shipment G; Chomerics
 
Descriptive Properties
CarrierG=Fiberglass, A=Aluminum
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics THERM-A-GAP 570 Thermally Conductive Gap Filler
Overview of materials for Silicone Rubber
Parker Chomerics V-THERM™ Thermally Conductive Elastomer
Aptek THERM-PAD 1100 Thermally conductive silicone pad
UBE Tyranno Grade A Ceramic Semi-Conductive Fiber

PCHOME001 / 28223

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.