MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) BLUESIL™ FB Silicone Gum
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: BLUESIL GUM™ FB is a dimethylsiloxane gum. It has been especially designed to manufacture HCR master batches, master batches of pigments, process additives, reinforcing and diluting fillers for silicone elastomers as well as plastics and organic elastomers.

Applications:

  • HCR Master batches with colored pigments and process additives
  • Master batches for plastics and organic elastomers
Features:
  • Stable after long storage
  • High consistency
  • Low volatile content
  • Translucent
  • Excellent heat stability, up to 200°C
  • High level of filler acceptance

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/cc
Volatiles <= 3.0 %
@Temperature 315 °C,
Time 900 sec
2 gm 10 mm Hg
Storage Temperature <= 40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
 
Descriptive Properties
AppearanceTranslucent
Consistency700-10001/10 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ GUM 795 Silicone Gum
Elkem (Bluestar Silicones) BLUESIL™ GUM 753 Silicone Gum
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 5000 Dimethylpolysiloxane Polymer
Elkem (Bluestar Silicones) BLUESIL™ WR 68 Water Repellent Treatment
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 50 Polydimethylsiloxanic Fluids

PBLUST123 / 191106

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.