MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals NOVAPOL® HE-Y449-AC HDPE Pipe Extrusion Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes:

Homopolymer

Features:

  • Medium molecular weight HDPE
  • High ESCR
  • Good toughness
  • Good chemical resistance
  • Good processability

Additives:

  • Processing antioxidant

Applications:

  • Corrugated tubing (up to 250 mm/10 in diameter)
  • Conduit

United States: NOVAPOL HB-Y449-AC resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D 792
ESCR 100% Igepal® >= 1000 hourF50, Condition B; ASTM D 1693
Melt Index of Compound 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ASTM D 2240
Tensile Strength, Yield 24.0 MPaTensile testing was conducted at a crosshead speed of 2 in/min; ASTM D 638
Elongation at Break 650 %Tensile testing was conducted at a crosshead speed of 2 in/min; ASTM D 638
Flexural Modulus 1140 MPaTangent; ASTM D 882
Izod Impact, Unnotched 1.10 J/cm
@Temperature 220 °C
In oxygen gas environment
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 124 °CASTM D 1525
Brittleness Temperature <= -70.0 °CASTM D 746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostalen CRP 100 BLACK (XL) High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Hostalen CRP 100 S RED High Density Polyethylene (HDPE), Pipe Grade
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Total XLS 12 B High Density Polyethylene - Pipes and Fittings
Formosa Plastics Formolene® HP4401 Pipe HDPE

PNOVB017 / 194625

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.