MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

DSM Somos® WaterShed® 11120 Water-resistant resin for stereolithography
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Description: DSM’s Somos® WaterShed 11120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly, parts created with Somos® WaterShed 11120 are nearly colorless, and look more like true, clear engineered plastic. In addition, Somos® WaterShed has been formulated with the DSM’s Somos® Oxetane Advantage™— an advanced chemistry platform that produces parts with outstanding water resistance and high dimensional stability.

Application: Somos® WaterShed 11120 offers many properties that mimic traditional engineering plastics, including ABS and PBT. This makes the material ideal for many applications in the automotive, medical and consumer electronic markets and include lenses, packaging, water flow analysis, RTV patterns, durable concept models, wind tunnel testing and quickcast patterns.

Information Provided by DSM Desotech Inc.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. North American leaders in delivering quick turnaround Rapid Prototyping and Additive Manufacturing solutions using all major 3D printing systems including SLA Stereolithography prototypes. Free online 3D printing quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc
@Temperature 25.0 °C
0.0405 lb/in³
@Temperature 77.0 °F
Water Absorption 0.35 %0.35 %ASTM D570-98
Viscosity 260 cP
@Temperature 30.0 °C
260 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 47.1 - 53.6 MPa6830 - 7770 psiASTM D638M
Elongation at Break 11 - 20 %11 - 20 %ASTM D638M
Elongation at Yield 3.3 - 3.5 %3.3 - 3.5 %ASTM D638M
Modulus of Elasticity 2.65 - 2.88 GPa384 - 418 ksiASTM D638M
Flexural Strength 63.1 - 74.16 MPa9150 - 10760 psiASTM D790M
Flexural Modulus 2.255 GPa327.1 ksiASTM D790M
Izod Impact, Notched 0.200 - 0.300 J/cm0.375 - 0.562 ft-lb/inASTM D256A
Graves Tear Strength 150.3 kN/m857.5 pliASTM D1004
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.4 - 3.5
@Frequency 1e+6 Hz
3.4 - 3.5
@Frequency 1e+6 Hz
ASTM D150-98
 3.7 - 3.9
@Frequency 1000 Hz
3.7 - 3.9
@Frequency 1000 Hz
ASTM D150-98
 3.9 - 4.1
@Frequency 60.0 Hz
3.9 - 4.1
@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 15.4 - 16.3 kV/mm391 - 414 kV/inASTM D149-97a
 
Thermal PropertiesMetricEnglishComments
CTE, linear  66.0 - 67.0 µm/m-°C
@Temperature -40.0 - 0.000 °C
36.7 - 37.2 µin/in-°F
@Temperature -40.0 - 32.0 °F
ASTM E831-00
 90.0 - 96.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
50.0 - 53.3 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831-00
 170 - 189 µm/m-°C
@Temperature 50.0 - 100 °C
94.4 - 105 µin/in-°F
@Temperature 122 - 212 °F
ASTM E831-00
 185 - 189 µm/m-°C
@Temperature 100 - 150 °C
103 - 105 µin/in-°F
@Temperature 212 - 302 °F
ASTM E831-00
Deflection Temperature at 0.46 MPa (66 psi) 45.9 - 54.5 °C115 - 130 °FASTM D648-98c
Deflection Temperature at 1.8 MPa (264 psi) 49.0 - 49.7 °C120 - 121 °FASTM D648-98c
Glass Transition Temp, Tg 39.0 - 46.0 °C102 - 115 °FASTM E1545-00
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.512 - 1.5151.512 - 1.515ASTM D542
 
Descriptive Properties
AppearanceOptically clear, near colorless
Dp (mm)5.5Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2)54Exposure that gives 0.254mm thickness
Ec (mJ/cm2)11.5Critical exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
3D Systems RenShape® SL 7820 Stereolithography Plastic
DSM Somos® NanoTool™ Resin for Stereolithography, UV & Thermal Postcure

PDSMT022 / 93542

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.