Description: DSM’s Somos® WaterShed 11120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly, parts created with Somos® WaterShed 11120 are nearly colorless, and look more like true, clear engineered plastic. In addition, Somos® WaterShed has been formulated with the DSM’s Somos® Oxetane Advantage™— an advanced chemistry platform that produces parts with outstanding water resistance and high dimensional stability. Application: Somos® WaterShed 11120 offers many properties that mimic traditional engineering plastics, including ABS and PBT. This makes the material ideal for many applications in the automotive, medical and consumer electronic markets and include lenses, packaging, water flow analysis, RTV patterns, durable concept models, wind tunnel testing and quickcast patterns. Information Provided by DSM Desotech Inc. |
 Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS. Axis Proto Inc. North American leaders in delivering quick turnaround Rapid Prototyping and Additive Manufacturing solutions using all major 3D printing systems including SLA Stereolithography prototypes. Free online 3D printing quotes at www.axisproto.comClick here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |