MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion FormaMet, EquaCast® Aluminium Bronze Cold Working Die Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: FormaMet is an aluminum bronze cold working die alloy used for the drawing or forming of stainless steel, low carbon steel and other materials. When used for deep drawing and forming applications offer the following advantages:
  • 39 HRc hardness minimizes wear and maximizes tool life
  • High galling resistance eliminates wrinkling and tearing of the deep drawn part
  • Very high wear resistance combined with excellent sliding properties

Information supplied by Brush Wellman Engineered Materials.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.251 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 39
Elongation at Break <= 0.5 %
Compressive Strength 220 ksi
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 264 BTU-in/hr-ft²-°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zirconium, Zr
8% Aluminum Bronze, UNS C61000
Ampco Metal AMPCO® 45 Nickel-Aluminum Bronze, Extruded and Drawn Rods, ≤ 25.4 mm.
AISI 321 Cast Stainless Steel, EN 10088-3
Ampco Metal AMPCO® 21 Aluminum Bronze, Round, ≤ 50.8 mm.

NBBC16 / 15326

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.