MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotchkote™ 426 Fusion Bonded Epoxy Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: 3M Scotchkote Fusion Bonded Epoxy Coating 426 is a one-part, heat curable, thermosetting epoxy coating designed for improved corrosion protection of reinforcing steel in severe marine and corrosive environments. The epoxy is applied to preheated steel as a dry powder which melts and cures to a uniform coating thickness. This bonding process provides excellent adhesion and coverage on concrete reinforcing steel bar and other steel members which have been prefabricated to any size or shape. Scotchkote 426 is resistant to cathodic disbondment and corrosive agents such as deicing salts, airborne slat spray, sea water, harsh chemicals, acid rain, carbonation, contaminated aggregate and concrete additives.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop >= 20
Abrasion 0.10[g] CS-17, 1000g weight, 5000 cycles; ASTM D1004
 19[mg] 1000g, 1000 cycles; ASTM A934

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schunk FF521 Resin Bonded Carbon
3M Scotchkote™ 206N XTRA LG Fusion Bonded Epoxy Coating
3M Scotchkote™ 412 Spray Grade Fusion Bonded Epoxy Coating
3M Scotchkote™ 412 Fusion Bonded Epoxy Coating
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade)

PMM35345 / 170092

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.