MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1403 Polyethersulfone (PES), Glass Fiber
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 20%Glass Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc1.51 g/ccASTM D 792
Water Absorption 0.40 %
@Time 86400 sec
0.40 %
@Time 24.0 hour
ASTM D 570
Additive Loading 20 %20 %Primary Additive
Linear Mold Shrinkage 0.0040 cm/cm
@Thickness 3.20 mm
0.0040 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ASTM D 785
Tensile Strength at Break 124 MPa18000 psiASTM D 638
Elongation at Break 2.9 %2.9 %ASTM D 638
Tensile Modulus 6.89 GPa1000 ksiASTM D 638
Flexural Strength 193 MPa28000 psiASTM D 790
Flexural Modulus 6.21 GPa900 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.20 mm
1.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.87 J/cm
@Thickness 3.20 mm
11.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cmASTM D 257
Dielectric Constant 3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 14.8 kV/mm375 kV/inShort Term; In Oil; ASTM D 149
Dissipation Factor 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
Dry; ASTM D 150
Arc Resistance 70 sec70 secASTM D 495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 28.8 µm/m-°C16.0 µin/in-°FE 831
Thermal Conductivity 0.303 W/m-K2.10 BTU-in/hr-ft²-°FThrough-plane; E 1530
Deflection Temperature at 0.46 MPa (66 psi) 221 °C430 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 216 °C420 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 343 - 377 °C650 - 710 °F
Mold Temperature 135 - 177 °C275 - 350 °F
Drying Temperature 149 °C
@Time 21600 sec
300 °F
@Time 6.00 hour
Moisture Content 0.040 %0.040 %
Dew Point -31.7 °C-25.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® E 2010 G4 20% Glass Filled PES
Gharda Chemicals GAFONE™ 3420GF PES, Glass Fiber-Reinforced
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced
Techmer ES HiFill® PES GF20 20% Glass Filled
Evonik VESTOSINT® 2070 natural color Polyamide 12

PQZWA2650 / 91275

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.