MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Rilsan® BZM 30 O TL PA11-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11 with 30% Glass Fiber Filler

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccISO 1183
 1.25 g/ccCond.; ISO 1183
Water Absorption 1.4 %Dry; Sim. to ISO 62
Moisture Absorption 0.500 %Dry; Sim. to ISO 62
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 235 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 74
@Time 15.0 sec
Dry; ISO 7619-1
Tensile Strength at Break 117 MPaCond.; ISO 527-1/-2
Elongation at Break 6.0 %Cond.; ISO 527-1/-2
Tensile Modulus 7300 MPaCond.; ISO 527-1/-2
Charpy Impact Unnotched 89.0 kJ/m²
@Temperature 23.0 °C
Cond.; ISO 179/1eU
 96.0 kJ/m²
@Temperature -30.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched 17.0 kJ/m²
@Temperature -30.0 °C
Cond.; ISO 179/1eA
 24.0 kJ/m²
@Temperature 23.0 °C
Cond.; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+13 ohm-cmCond.; IEC 60093
Surface Resistance 1.00e+14 ohmCond.; IEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 4.0
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 45.0 kV/mmCond.; IEC 60243-1
Dissipation Factor 0.021
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.0578
@Frequency 100 Hz
Dry; IEC 60250
Comparative Tracking Index 600 VCond.; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°CDry; ISO 11359-1/-2
Melting Point 189 °C10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 180 °CDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 175 °CDry; ISO 75-1/-2
Vicat Softening Point 170 °C50°C/h 50N; Dry; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
Oxygen Index 22 %Dry; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 10724
Hold Pressure 22.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
%Bio-Based98ASTM D6866
Bio-BasedYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsInjection Molding
Release agentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsan® BSR 30 PA11-CF30
Arkema Rilsan® BZM 30 BLACK TL Nylon 11, 30% Glass Fiber Filled
Arkema Rilsan® BUM 30 O PA11-GB30
Arkema Rilsan® Clear G300 HI PA
Arkema Rilsan® Clear G850 Rnew® PA

PARKF909 / 193646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.