MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Description: PELLETHANE® 2103-75D UV stabilized, polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications include: Film, Tubing and belting, Geophysical wire and cable jacketing, Cell phones and PDA overmolding

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0080 cm/cm
@Thickness 1.59 mm
plaque
Linear Mold Shrinkage, Transverse 0.0030 - 0.0070 cm/cm
@Thickness 1.59 mm
plaque
Melt Index of Compound 28 g/10 min
@Load 5.00 kg,
Temperature 224 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72 - 80ASTM D2240
Tensile Strength, Ultimate 40.0 MPaASTM D412
Elongation at Break 380 %ASTM D412
50% Modulus 0.0305 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.0313 GPa
@Strain 100 %
ASTM D412
Flexural Modulus 190000 psiASTM D790
Tear Strength 257 kN/mDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 55H-22 wheel (coarser); ASTM D1044
Tensile Set 40 %Elongation Set After Break; ASTM D412
 
Thermal PropertiesOriginal ValueComments
CTE, linear 88.7 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Vicat Softening Point 116 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature 204 - 221 °COptimum Extrusion Temperature
Melt Temperature 210 - 227 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Delrin Delrin® 100 BK602 POM
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)
Dow Pellethane® 2354-65D Polyurethane Elastomer, Polyester Polycaprolactone Based

PDW297 / 34465

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.