MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik SITREN® P 750 Water repellent
Categories: Other Engineering Material

Material Notes: Product description: SITREN® P 750 is a highly efficient water repellent based on modified silanes/siloxanes on in powder form.

Applications: SITREN® P 750 may be used in a variety of cementitious drymix applications where the application of conventional liquid water repellents is not feasible or desired, e. g.:

  • Tile grouts
  • Plasters
  • Renders
  • Sealing slurries
Properties/Benefits: As well as excellent water repellence and beading SITREN® P 750 provides:
  • Long term performance
  • Improved soil release properties
  • Good free-flow behavior
  • Low dust formation
  • Almost no wetting delay
  • No incompatibility with other additives
  • Good alkaline stability

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Appearancewhite powder
Content50%active

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Aluminum Nitride (TiAlN) PVD Coating
Evonik TEGOPREN® 5878 Additive
Evonik SITREN® PSR 100 Additive
Evonik SITREN® AirVoid® 354 Surfactant
Evonik Protectosil® Degadeck® CSS Surface Treatment

PEVONIM178 / 197382

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.