MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPC 4481WZ Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: TOTAL Petrochemicals Polypropylene 4481WZ is a nucleated impact copolymer with a Melt Flow index of 4.0 g/10 min.

TOTAL Polypropylene 4481WZ is characterized by a good stiffness/impact balance coupled with high creep resistance. This grade has been developed for sheet extrusion and thermoforming applications requiring good mechanical properties and aesthetic appearance.

Total Polypropylene 4481WZ has been specially formulated with an additive for excellent antistatic properties as well as good surface appearance and mold release.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccASTM D1505
Melt Flow 4.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 34.0 MPaASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 1650 MPaASTM D790
Izod Impact, Notched 2.60 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 - 165 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 115 °Cpressure unspecified; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet
Total PPC 4280W Polypropylene, Impact Copolymer
Total PPC 4524WZ Polypropylene, Impact Copolymer
Ineos N02J-00 Polypropylene Impact Copolymer
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade

PTOTAL863 / 130588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.