MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel SUPERELSO® 960 HLE Steel for Welded and Weight-Saving Structures
Categories: Metal; Ferrous Metal; Carbon Steel; Medium Carbon Steel

Material Notes: Description: SUPERELSO® 960 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 960 N/mm² (140 KSI), SUPERELSO® 960 enables to make weight savings or support higher stresses and thus carry higher payload. With a good quality of steel making process, an adapted chemical analysis (low alloying content) and an excellent precision in Industeel's fabrication process (thickness tolerance, uniform mechanical characteristics), SUPERELSO® 960 is easy to machine, to bend and to weld which simplify production and maintenance. By using S SUPERELSO® 960 and thus thinner plate in welded structures, you limit preheating conditions, you decrease quantity of consumables, welding time and so production costs.

Information provided by manufacturer.

Key Words: EE 960 TIIK4 according to NFA 36-204, S 960 QL according to EN 10137-2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1000 - 1130 MPa145000 - 164000 psiTypical
Tensile Strength, Yield >= 960 MPa
@Strain 0.2 %
>= 139000 psi
@Strain 0.2 %
Elongation at Break >= 10 %>= 10 %
 13 %13 %
Charpy Impact  >= 30.0 J
@Temperature -20.0 °C
>= 22.1 ft-lb
@Temperature -4.00 °F
Transverse
 >= 40.0 J
@Temperature -20.0 °C
>= 29.5 ft-lb
@Temperature -4.00 °F
Longitudinal
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.040 - 0.070 %0.040 - 0.070 %
Carbon, C 0.18 %0.18 %
Chromium, Cr 0.80 %0.80 %
Copper, Cu 0.30 %0.30 %
Iron, Fe 93.91 - 93.94 %93.91 - 93.94 %As remainder
Manganese, Mn 1.5 %1.5 %
Molybdenum, Mo 0.60 %0.60 %
Nickel, Ni 2.0 %2.0 %
Phosphorus, P 0.025 %0.025 %
Silicon, Si 0.50 %0.50 %
Sulfur, S 0.015 %0.015 %
Vanadium, V 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ThyssenKrupp XABO® 960 Structural Steel
Industeel SUPERELSO® 890 HLE Steel for Welded and Weight-Saving Structures
Silberline Sparkle Silvet® 960-25-E
Aluminum 356.0-T71, Sand Cast
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-6 (UNS S20153)

NINDUST47 / 17585

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.