MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Riteflex® 640A TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: 40 Shore D Hardness 12,300 PSI flexural modulus

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Absorption 0.50 %
@Temperature 22.8 °C
0.50 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Viscosity 351100 cP351100 cP
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inASTM D955
 0.012 - 0.014 cm/cm0.012 - 0.014 in/inISO 294-4
Melt Flow 8.0 - 12 g/10 min8.0 - 12 g/10 minASTM D1238
 10 g/10 min
@Load 2.16 kg,
Temperature 220 °C
10 g/10 min
@Load 4.76 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4040ASTM D2240
 4040
 404015 sec; ISO 868
 4040ISO 868
Tensile Strength at Break 17.0 MPa2470 psi50mm/min; ISO 527-2/1A
 20.7 MPa3000 psiASTM D638
Tensile Stress at Strain  3.00 MPa
@Strain 5.0 %
435 psi
@Strain 5.0 %
ISO 527-1/2
 5.00 MPa
@Strain 10 %
725 psi
@Strain 10 %
ISO 527-1/2
 8.00 MPa
@Strain 50 %
1160 psi
@Strain 50 %
ISO 727-1/2
 8.00 MPa
@Strain 50 %
1160 psi
@Strain 50 %
ISO 527-2/1A
Elongation at Break >= 300 %>= 300 %
 480 %480 %ASTM D638
Tensile Modulus 0.0750 GPa10.9 ksi50mm/min; ISO 527-2/1A
 0.0924 GPa13.4 ksiASTM D638
Flexural Strength 5.00 MPa725 psiISO 178
 3.00 MPa
@Strain 3.5 %
435 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 0.0700 GPa10.2 ksiISO 178
 0.0848 GPa12.3 ksiASTM D790
 0.115 GPa
@Temperature -40.0 °C
16.7 ksi
@Temperature -40.0 °F
ISO 178
 0.154 GPa
@Temperature -40.0 °C
22.4 ksi
@Temperature -40.0 °F
ASTM D790
Resilience 5959Bayshore, %; ASTM D2632
 5959Bayshore, %
Flex Crack Resistance >= 1.00e+6>= 1.00e+6Ross flex
Izod Impact, Notched NBNBASTM D256
 NBNB
Izod Impact, Notched (ISO)  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched NBNBISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
Tear Strength 84.0 kN/m479 pliISO 34-1
 110 kN/m630 pliASTM D1004
 126 kN/m720 pliASTM D624
Taber Abrasion, mg/1000 Cycles 9090ASTM D4060
Compression Set <= 1.5 %<= 1.5 %ASTM D395
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+12 ohm-cm5.00e+12 ohm-cmIEC 60093
 5.00e+12 ohm-cm5.00e+12 ohm-cmASTM D257
Surface Resistance 3.00e+15 ohm3.00e+15 ohmIEC 60093
Dielectric Constant 4.7
@Frequency 1e+6 Hz
4.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 11.8 kV/mm300 kV/inshort term; ASTM D149
 13.0 kV/mm330 kV/inIEC 60243-1
Dissipation Factor 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VASTM D3638
 >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 220 µm/m-°C122 µin/in-°FISO 11359-2
Melting Point 170 °C338 °F10°C/min; ISO 11357-1,-2,-3
 180 °C356 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C133 °FISO 75-1, -2
Vicat Softening Point 136 °C277 °FASTM D1525
Brittleness Temperature -78.0 °C-108 °FISO 974
Glass Transition Temp, Tg -65.0 °C-85.0 °FASTM D3418
Flammability, UL94 HBHB
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 55.0 °C68.0 - 131 °Fcavity
 170 - 205 °C338 - 401 °Fhot runner
Feed Temperature 160 - 180 °C320 - 356 °F
Zone 1 160 - 180 °C320 - 356 °F
Zone 2 170 - 200 °C338 - 392 °F
Zone 3 170 - 200 °C338 - 392 °F
Zone 4 170 - 205 °C338 - 401 °F
Die Temperature 170 - 205 °C338 - 401 °F
Melt Temperature 170 - 205 °C338 - 401 °F
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 4.00 hour4.00 hour
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing typeInj/Blow/Ext

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Riteflex® 655A TPC, Unfilled
Celanese Riteflex® 663 TPC, Unfilled
Celanese Riteflex® 425 TPC, Unfilled
Celanese Riteflex® 655HS TPC, Unfilled
Celanese Riteflex® 435 TPC, Unfilled

PHCQ451 / 178906

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.