MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: TSE326 is a one-component, heat curing silicone adhesive which offers extended performance at temperatures exceeding 200C. A flowable material with primerless adhesion to many substrates, it is suitable for assembly and gasketing where a flowable consistency is required. TSE 326 requires a minimum cure temperature of 100C and offers very low linear shrinkage and an improved thermal conductivity of 0.29 W/m K. Reddish brown in color.

Key Performance Properties:

  • One component product-no mixing required
  • Fast cure at elevated temperatures
  • Primerless adhesion to many types of substrates
  • Low linear shrinkage
  • Excellent heat resistance
  • Outstanding dielectric properties

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/cc
Viscosity 28000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 43
Tensile Strength, Ultimate 35.0 kg(f)/cm²
Elongation at Break 170 %
Adhesive Bond Strength 284 psiAluminum to aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+15 ohm-cm
Dielectric Constant 3.3
Dielectric Strength 21.97 kV/mm
Dissipation Factor 0.020
 
Thermal PropertiesOriginal ValueComments
CTE, linear 170 µm/m-°C
@Temperature 20.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 150 °C
 0.750 hour
@Temperature 125 °C
 2.00 hour
@Temperature 100 °C
 
Descriptive Properties
ColorReddish Brown

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials TSE3261-G Heat Resistant Silicone Adhesive
Momentive Performance Materials TSE322B Heat-Curing Silicone Adhesive, Black
Momentive Performance Materials TSE3221 Flowable, Heat Cured One Component Silicone Adhesive
Henkel Loctite® 5420 Heat Cure Form-In-Place Electrically Conductive Silicone Sealant
Henkel Loctite® Output™ 5404 Heat Cure Silicone

PGESIL067 / 41058

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.