MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering S70L Conductive Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Tan coloured, Silicone Rubber, 66-75 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber. Equivalent to Mil G 83528 Type D.

Applications: Specially compounded to offer excellent physical and electrical properties over an effective temperature range of -50° to +160°C. It has good resistance to chemicals and weathering. Resistance to mineral based oils and greases is poor, but it can withstand limited splash contact.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70°IRHD; ASTM D1415
Tensile Strength, Yield >= 1.25 MPaASTM D412
Elongation at Break >= 100 %ASTM D412
Compression Set 30 %
@Temperature 70.0 °C,
Time 252000 sec
ASTM D395
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.0080 ohm-cmMil G 83528
Shielding Effectiveness 70 dB@ 200 kHz; Mil Std 285
 100 dB@ 2 GHz; Mil Std 285
 100 dB@ 10 GHz; Mil Std 285
 105 dB@ 500 MHz; Mil Std 285
 110 dB@ 100 MHz; Mil Std 285
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °C
Minimum Service Temperature, Air -50.0 °C
Flash Point >= 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® L-R1-MHI Antistatic, Black, Electrically Conductive Nylon 12
Rogers Corporation Bisco® EC-2040 Conductive Silicone
Asahi Kasei TENAC™-C C84 Copolymer Acetal (POM), Electrically Conductive
A. Schulman ComAlloy E-16903B Nylon 6/6, Electrically Conductive - Stainless Steel Fiber Filled
Aluminum 2124-T351

PPRECI267 / 57991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.