MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 199 X 138766 Z EG Polypropylene (PP); Permanently Static Dissipative - ESD Protection - FDA Compliant Ingredients - Extrusion Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D 792
Melt Flow 3.0 - 6.0 g/10 min
@Load 2.16 kg
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2300 psiASTM D 638
Elongation at Break >= 10 %ASTM D 638
Tensile Modulus 100 ksiASTM D 638
Flexural Strength 3000 psiASTM D 790
Flexural Modulus 100 ksiASTM D 790
Izod Impact, Notched 13.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+7 - 9.90e+8 ohm-cmASTM D 257
Surface Resistivity per Square 1.00e+8 - 9.90e+9 ohmASTM D 257; ESD STM11.11
Static Decay <= 2.0 secFTMS101C; 4046.1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 340 - 400 °F
Drying Temperature 175 °F
@Time 7200 sec
Moisture Content <= 0.020 %
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE)
RTP Company RTP 199 X 123298 Polypropylene (PP); High Impact - Permanently Static Dissipative - ESD Protection - UV Stabilized
RTP Company RTP 199 X 125315 Polypropylene (PP); Permanently Anti-static - ESD Protection
Avient Trilliant™ HC FPO PPC-10G Natural PP Copolymer with 10% Glass Fabric
Avient Therma-Tech™ NN-3000 TC Polyamide 66 (Nylon 66)

PQZRA30008 / 206119

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.