MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dimethyl Formamide (HCON(CH3)2; N,N-dimethylformamide; DMF)
Categories: Fluid; Solvent

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9487 g/cc
@Temperature 20.0 °C
Viscosity 0.794 cP
@Temperature 25.0 °C
Molecular Weight 73.09 g/mol
Vapor Pressure 0.09869 atm
@Temperature 83.9 °C
Surface Tension 17.34 dynes/cm
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Temperature 376.48 °C
Critical Density 0.279 g/cc
Critical Molar Volume 262 cm³/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 108.1 J/gEnthalpy of fusion at normal melting point
Heat of Vaporization 641.5 J/g
@Temperature 25.0 °C
Enthalpy of vaporization
Thermal Conductivity 0.184 W/m-K
@Temperature 25.0 °C
Melting Point -60.48 °CAt atmospheric pressure (760 torr)
Boiling Point 39.9 °Cat 10 torr
 149.56 °C
@Pressure 0.101 MPa
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.368
@Wavelength 589.3 nm
nD
 
Descriptive Properties
CAS registry number (CARN)68-12-2
Chemical FormulaC3H7NO
UN Number2265
UV cut-off (nm)270

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Isopropanol ((CH3)2CHOH; 2-Propanol)
Ethylene glycol, C2H6O2

VORG016 / 74527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.