MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil C4LL 50026.19 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: ExxonMobil™ C4LL 50026.19 resin is a narrow molecular weight ethylene 1-butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in freezer applications for food packaging.

Availability: Latin America and North America

Applications:

  • Protective Caps
  • Closures and Dispensers
  • Freezer Lids
  • Housewares

Information provided by ExxonMobil

Key Words: ExxonMobil™ LLDPE LL 6201.19
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ExxonMobil method
ESCR 10% Igepal® 40.0 hour40.0 hourF50; ASTM D1693B
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 13.8 MPa2000 psiASTM D638
Elongation at Break 157 %157 %ASTM D638
Flexural Modulus 0.441 GPa
@Strain 2 %
64.0 ksi
@Strain 2 %
Secant; ASTM D638
Flexural Modulus, 1% Secant 510 MPa74000 psiASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 121 °C<= 250 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 82.0 °C180 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ FSU-105-E Concentrate Based In LDPE
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
ExxonMobil Exceed™ Flow m 0527.MC Film Grade Hexene LLDPE
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin
ExxonMobil LL 1001XKI Film Grade Butene LLDPE

PEX99169 / 175405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.