Product Description: ExxonMobil™ C4LL 50026.19 resin is a narrow molecular weight ethylene 1-butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in freezer applications for food packaging. Availability: Latin America and North America Applications: - Protective Caps
- Closures and Dispensers
- Freezer Lids
- Housewares