MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® FST2 Thermoplastic  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Fully compliant aviation sheet

KYDEX® FST2 is a proprietary, high performance non-PVC thermoplastic sheet specifically formulated to meet all Boeing and Airbus Flammability, OSU Heat Release, Smoke, and Toxicity requirements for aircraft interior components.

KYDEX® FST2 meets the flammability and smoke development requirements outlined in Federal Aviation Regulations (FAR) 25.853 paragraphs (a) and (d) and the toxicity requirements for Airbus (ABD0031) and Boeing (BSS7239). Its wide processing window and ease of thermoforming makes it ideal for complex parts.

Suggested Applications:

  • Seat parts
  • Armrests
  • Bulkhead laminates
  • Window shades
  • Molding strips
  • Passenger service units
  • Tray tables
  • Monitor shrouds
  • Kick panels

Features:

  • Meets the stringent requirements of FAR 25.853(d) in all thicknesses and colors
  • Compliant to ABD0031 and BSS7239 toxicity specifications
  • Excellent formability and fabrication characteristics
  • Allows for tight tolerance control
  • Low gloss
  • Excellent UV resistance
  • Excellent chemical resistance
  • Lighter weight
  • Available in P3 – Velour Matte

Values based upon 0.125 in (3.17 mm) sheet unless otherwise specified

Pre-drying of KYDEX® FST2 is required prior to thermoforming in order to remove moisture from the sheet.

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Moisture Absorption 0.200 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ASTM D785
Tensile Strength 58.6 MPaASTM D638
Tensile Modulus 2868 MPaASTM D638
Flexural Strength 90.3 MPaASTM D790
Flexural Modulus 2910 MPaASTM D790
Compressive Yield Strength 73.1 MPaASTM D695
Compressive Modulus 2860 MPaASTM D695
Ultimate Bearing Strength 208.2 MPaASTM D953
Bearing Yield Strength 31.7 MPa4% deflection; ASTM D953
Shear Strength 45.1 MPaASTM D732
Izod Impact, Notched 254 J/mASTM D256
Gardner Impact 37.3 JASTM D5420
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 23.8 kV/mmoil; ASTM D148
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 24.0 µin/in-°FASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 250 °FUnannealed/Annealed; ASTM D648
 
Descriptive Properties
FlammabilityPassFAR 25.853(a)(ii); Vertical Burn, 12 sec; all thicknesses
 PassFAR 25.853(a)(i); Vertical Burn, 60 sec; all thicknesses
 PassFAR 25.853(d) Part IV; OSU Heat Release; all thicknesses
 PassFAR 25.853(d) Part V; NBS Smoke Density; all thicknesses
 PassABD0031; Airbus Toxic Gas Generation; all thicknesses
 PassBSS 7239; Boeing Toxic Gas Generation; all thicknesses

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® 410 ABS/PVC
SEKISUI SPI KYDEX® 430 ABS/PVC
SEKISUI SPI KYDEX® 2200LT Thermoplastic
SEKISUI SPI KYDEX® T Thermoplastic
SEKISUI SPI KYDEX® 100 Polymer Alloy Sheet

PSEKIS029 / 185854

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.