MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:
  • Keyboard Covers
  • Outsoles of Soccer Shoes
  • Wire and Cable
  • Airbags
  • Sheets and Film
  • Hoses and Tubing
  • Shoe Components
  • Fire Hoses

Information provided by SK Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 96ASTM D2240
Hardness, Shore D 53ASTM D2240
Tensile Strength, Ultimate 500 kg(f)/cm²ASTM D412
Elongation at Break 500 %ASTM D412
100% Modulus 2.30 ksi
@Strain 100 %
ASTM D412
300% Modulus 5.10 ksi
@Strain 300 %
ASTM D412
Resilience 37Vertical Rebound; ASTM D2632
Tear Strength 140 kg(f)/cmDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 30H18 wheel, 1000g load; ASTM D1044
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 130 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature 205 °CTransition Temperature
 205 °CMetering Temperature
Middle Barrel Temperature 200 °C
Nozzle Temperature 210 °C
Zone 1 374 °F
Zone 2 383 °F
Zone 3 392 °F
Zone 4 401 °F
Adapter Temperature 205 °C
Die Temperature 401 °FTip
 410 °FBody
Mold Temperature 20.0 - 40.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wanhua Chemical Wanthane® WHT-2180 Polycaprolactone Based TPU
RTP Company RTP 1200 T-70A UV Ether-based Thermoplastic Polyurethane Elastomer (; UV Stabilized
RTP Company RTP 1200 T-70A Z NATURAL Ether-based Thermoplastic Polyurethane Elastomer (; Translucent
BASF Elastollan® 1175AW Polyether Type Polyurethane Elastomer
C.O.I.M. LARIPUR® LPR2102-85AE Polycaprolactone Ester Polyurethane

PSK031 / 67766

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.