MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PolyMirae Moplen EP548P Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen EP548P is a nucleated heterophasic copolymer, suitable for injection molding applications, and contains an anti-static agent. It exhibits a high stiffness combined with a medium fluidity. Moplen EP548P is extensively used in houseware, furniture, cylindrical containers and crates. EP548P resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.

Product Features: Heterophasic Copolymer/Excellent Antistatic/Good Impact and Stiffness Balance/Food Contact Acceptable/Nucleated/Easy processability

Typical Applications: Crates/Furniture/Housewares/Opaque containers

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 15000 kg(f)/cm²ASTM D790
Izod Impact, Notched 6.00 kg-cm/cm
@Temperature -20.0 °C
ASTM D256
 16.0 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °CASTM D648
Vicat Softening Point 147 °CASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Adstif HA5034 Injection Molding Grade Polypropylene
PolyMirae Moplen EP5015 Injection Molding Grade Polypropylene
LyondellBasell Moplen EP548P Polypropylene, Impact Modified; Molded/Extruded
PolyMirae Moplen EP500M Injection Molding Grade Polypropylene
PolyMirae Moplen EP452R Injection Molding Grade Polypropylene

PMIRAF27 / 183248

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.