MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil C4LL 1018.31 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: ExxonMobil™ C4LL 1018 Series are butene LLDPE blown film resins that have good drawdown. Films made from ExxonMobil™ C4LL 1018 resins exhibit good tensile and toughness properties.

Availability: Latin America and North America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Agricultural Film
  • Bag in Box
  • Barrier Food Packaging
  • Blown Film
  • Bread Bags
  • Food packaging
  • Form Fill and Seal Packaging
  • Freezer Film
  • Garment Film
  • General Packaging
  • Heavy Duty Bags
  • Ice Bags
  • Industrial Liners
  • Industrial Packaging
  • Lamination Film
  • Liners
  • Multilayer Packaging Film
  • Packaging Films
  • Produce Bags
  • Refuse Bags
  • Shoppers
  • Stand Up Pouches
  • Trash Bags

Information provided by ExxonMobil

Key Words: LLDPE LL 1001X31
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccExxonMobil method
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 9.00 lb (f)
Film Tensile Strength at Yield, MD 1400 psiASTM D882
Film Tensile Strength at Yield, TD 1400 psiASTM D882
Film Elongation at Break, MD 570 %ASTM D882
Film Elongation at Break, TD 870 %ASTM D882
Puncture Energy 25.0 in-lbExxonMobil Method
Elmendorf Tear Strength MD 90 gASTM D1922
Elmendorf Tear Strength TD 450 gASTM D1922
Dart Drop Test 90.0 gASTM D1709A
Film Tensile Strength at Break, MD 7300 psiASTM D882
Film Tensile Strength at Break, TD 5200 psiASTM D882
1% Secant Modulus, MD 28000 psiASTM D882
1% Secant Modulus, TD 33000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 250 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 99.0 °C
 
Optical PropertiesOriginal ValueComments
Haze 14 %ASTM D1003
Gloss 45 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force10 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil C4LL 20025.17 Linear Low Density Polyethylene Resin
ExxonMobil Escorene® LL-6101 LLDPE, Injection Grade
DuPont Teijin Films Mylar® LB Polyester Film, 92 Gauge (23 µm)
ExxonMobil HD 5404 High Density Polyethylene Resin
ExxonMobil HD 6207 High Density Polyethylene Resin

PEX99141 / 175377

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.