MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis BorSafe™ ME3440 Black Medium Density Polyethylene for Pressure Pipes
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Extruded

Material Notes: ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Borstar technology. Well dispersed carbon black gives outstanding UV resistance. Long-term stability is ensured by an optimized stabilization system.

ME3440 is recommended for pressure pipe systems in the application fields of drinking water, natural gas, pressure sewerage, relining, sea outfall and industrial, particularly where flexibility and coilability is of importance. It also shows excellent resistance to rapid crack propagation and slow crack growth. Thanks to the structure, it gives outstanding extrudability, compared to conventional PE80 products.

Former trade name for this product was Borstar®.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccBase Resin; ISO 1183
 0.951 g/ccCompound; ISO 1183
ESCR 10% Igepal® >= 5000 hourASTM D1693-A
Carbon Black Loading >= 2.0 %ASTM D1603
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 0.85 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2755 psiAt 50 mm/min; ISO 527-2
Elongation at Break 600 %ISO 527-2
Elongation at Yield 10 %ISO 527-2
Tensile Modulus 0.800 GPaAt 1 mm/min; ISO 527-2
Charpy Impact, Notched 0.200 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -70.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Front Barrel Temperature 180 - 210 °C
Die Temperature 392 - 410 °F
Melt Temperature 200 - 220 °C
Head Temperature 200 - 210 °C
 
Descriptive Properties
Resistance to Rapid Crack Propagation, BAR7ISO 13477, Pc at 0°C, S4 / pipe size 250 mm SDR 11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BorSafe™ HE3490-LS Black High Density Polyethylene for Pressure Pipes
Borealis BorSafe™ HE3470-LS Black HDPE Compound for Pressure Pipes
Overview of materials for Medium Density Polyethylene (MDPE), Molded
Borealis BorSafe™ ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes
Borealis BorSafe™ ME3445 Medium Density Polyethylene

PBOREA133 / 27440

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.