MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling Trovidur® PHT PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Product characteristics:
  • Uniform physical properties
  • Continuous service temperature up to 90°C
  • High resistance to acids, lyes and salt solutions
Product applications:
  • Chemical engineering and tank building
  • Clean room and semi conductor industry
  • Ventilation technology

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.64 g/ccDIN EN ISO 1183-1
Water Absorption <= 0.20 %DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75DIN EN ISO 868
Tensile Strength, Yield 60.0 MPaDIN EN ISO 527
Elongation at Break 15 %DIN EN ISO 527
Modulus of Elasticity 3.00 GPaDIN EN ISO 527
Izod Impact, Notched (ISO) 4.00 kJ/m²DIN EN ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+13 ohmDIN EN 62631-3-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 80.0 µm/m-°CDIN 53752
Thermal Conductivity 0.130 W/m-KDIN 52612-1
Maximum Service Temperature, Air 90.0 °Clong term
Vicat Softening Point 107 °CDIN EN ISO 306, Vicat B
Minimum Service Temperature, Air -10.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Colorite Polymers 2007NAT Rigid PVC
Colorite Polymers 2007F Rigid PVC
Colorite Polymers 2002 Rigid PVC
Axiall Suprel® SVA 9412 Rigid PVC, Molding
Axiall Suprel® SVA 9301 Rigid PVC, Molding

PROCH9367 / 233069

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.