MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® HP4401 Pipe HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: High Density Hexene Copolymer

Applications: Potable water, industrial mining, oil and gas gatherings

Formolene HP4401 is a high performance copolymer that is designed for the most demanding requirements of pressure pipe applications. It has good long-term hoop strength performance, very high melt strength, outstanding toughness even at low temperatures.

Produced using licensor formulation for HHM TR-480Z. Licensor does not warrant or imply that this product meets their specifications for HHM TR-480Z.

Formolene HP4401 meets all the requirements of ASTM D4976-PE225. It also meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520 for food packaging.

Nominal properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Physical properties are typical of product but do not reflect normal testing variance and therefore should not be used for specification purposes.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.944 g/ccNatural; ASTM D1505
 0.955 g/ccBlack; ASTM D1505
ESCR 100% Igepal® >= 1000 hourCondition A,B,C, F50; ASTM D1693
Melt Flow 0.11 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Condition E; ASTM D1238
High Load Melt Index 12 g/10 min
@Load 21.6 kg,
Temperature 190 °C
Condition F; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
PENT 150 hourASTM F1473
Tensile Strength at Break 5000 psi2" (50mm) per min.; ASTM D638 Type IV
Tensile Strength, Yield 3200 psi2" (50mm) per min.; ASTM D638 Type IV
Elongation at Break >= 500 %2" (50mm) per min.; ASTM D638
Flexural Modulus 110000 psiASTM D3350
 140000 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -130 °FASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
LyondellBasell Petrothene® LP500200 High Density Polyethylene (Sheet & Profile Grade)
ExxonMobil Paxon™ BA46-055 Blow Molding Resin
ExxonMobil Paxon™ BU46-060 High Density Polyethylene (HDPE), Copolymer Film Grade

PFPCPE24 / 38831

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.