MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPC 4524WZ Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: TOTAL Petrochemicals Polypropylene 4524WZ is a nucleated high impact copolymer with a Melt Flow index of 7 g/10 min.

TOTAL Polypropylene 4524WZ is characterized by significantly improved impact resistance, while maintaining excellent antistatic properties and good processability.

Total Polypropylene 4524WZ has been developed specifically for the injection molding of baskets, pails, toys and any articles requiring extra toughness.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccASTM D1505
Melt Flow 7.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 26.0 MPaASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 1180 MPaASTM D790
Izod Impact, Notched 70.0 J/m
@Temperature -20.0 °C
ASTM D256
 188 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 - 165 °CTOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CPressure unspecified; ASTM D648
Vicat Softening Point 148 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPC 4624WZ Polypropylene, Impact Copolymer
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet
Total PPC 4280W Polypropylene, Impact Copolymer
Total PPC 4481WZ Polypropylene, Impact Copolymer
Total PPR 3221 Random Copolymer Polypropylene, Blow Molding and Sheet Extrusion

PTOTAL866 / 130591

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.