MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond EP21AOLV-2LO Two Part, Thermally Conductive and Electrically Insulative Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond Polymer Adhesive EP21AOLV-2LO is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant, coating and encapsulant. This versatile system will adhere to a wide variety of substrates including metals, glass, ceramics and many plastics. EP21AOLV-2LO has a convenient, one to one mix ratio by weight. Its ability to flow readily and smoothly is another benefit. It is also an excellent adhesive and coating, but realistically, the system is mostly used for potting and encapsulating. In fact, it can be used in larger potting applications because it has very low exotherm when curing. EP21AOLV-2LO resists a wide range of chemicals including water, oils, fuels and many solvents. The service temperature range for this epoxy is -60°F to +250°F. EP21AOLV-2LO has a low coefficient of thermal expansion and enhanced dimensional stability, along with both a high modulus and compressive strength. Its most significant feature is that it meets ASTM E595 requirements for NASA low outgassing. This combination of properties makes EP21AOLV-2LO highly desirable for a wide variety of applications. The color of Part A is gray; the color of Part B is off-white. EP21AOLV-2LO is widely used in the aerospace, electronic, electro-optical and optical industries where low outgassing, superior thermal conductivity and electrical insulation are critical requirements.

Product Advantages:

  • Convenient mixing: non-critical equal weight ratio.
  • Easy application: readily flowable when potting; brushable when bonding.
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures.
  • High bonding strength to a wide variety of substrates.
  • Low coefficient of expansion, low shrinkage and superb dimensional stability.
  • Superior durability, thermal shock and chemical resistance.
  • Outstanding thermal conductivity, over 10 BTU•in/ft2 •hr•°F.
  • Excellent electrical insulation properties.
  • Very low exotherm; suitable for larger castings.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 1500 - 3000 cP1500 - 3000 cPPart A
 55000 - 125000 cP55000 - 125000 cPPart B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Strength at Break >= 34.5 MPa
@Temperature 23.9 °C
>= 5000 psi
@Temperature 75.0 °F
Tensile Modulus >= 3.10 GPa
@Temperature 23.9 °C
>= 450 ksi
@Temperature 75.0 °F
Compressive Strength >= 103 MPa>= 15000 psi
Shear Strength >= 8.27 MPa>= 1200 psiAl/Al, bond
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cm
Dielectric Constant 4.5
@Frequency 60 Hz,
Temperature 25.0 °C
4.5
@Frequency 60 Hz,
Temperature 77.0 °F
Dielectric Strength >= 15.7 kV/mm
@Thickness 3.17 mm
>= 400 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 22.0 - 25.0 µm/m-°C12.2 - 13.9 µin/in-°F
Thermal Conductivity >= 1.44 W/m-K>= 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 240 min
@Temperature 93.3 °C
2.00 - 4.00 hour
@Temperature 200 °F
 4320 - 5760 min
@Temperature 23.9 °C
72.0 - 96.0 hour
@Temperature 75.0 °F
Pot Life 4.0 - 6.0 min4.0 - 6.0 min100 gram mass
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original, unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)1:1by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP21TDC-2AN Two Component, Flexibilized, Highly Thermally Conductive, Electrically Insulating Epoxy Resin
Master Bond EP21NDFG Two component epoxy compound for high performance applications
Master Bond EP21SC-1 Two Component Epoxy Resin System
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Master Bond EP42HT-2AO Two Component, Thermally Conductive, Heat Resistant Epoxy

PMASTB308 / 149555

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.